Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 102 kV/mm | 2580 kV/in | Z Direction; IPC-TM-650 2.5.6.2 |
Rogers Corporation XT/duroid™ 8100 0.002" Woven Glass Reinforced Thermoplastic Circuit Material XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81.. |