Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.27 kV/mm | 210 kV/in | |
Saint-Gobain CHR® M99 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Strength | 8.27 kV/mm | 210 kV/in | |
Dow Corning SC 102 White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning |
|||
Dielectric Strength | 8.27 kV/mm | 210 kV/in | |
Dow Corning 340 Heat Sink Compound White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning |