Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.87 - 16.0 kV/mm | 200 - 406 kV/in | Average value: 15.3 kV/mm Grade Count:11 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | |
CE Phenolic Laminate Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular (Short Time) |
Industrial Laminates/Norplex MC223 Cotton Fabric Description: Grade MC223 is a medium weave cotton phenolic composite that is specifically formulated to meet MIL-P-18324.Typical applications include pintle and stave-type bearings for rudder shafts.. |
|||
Dielectric Strength | >= 7.87 kV/mm | >= 200 kV/in | ASTM D149 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | |
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base Single component system with a paint consistency. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | |
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D149 |
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic a.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Solvent Resistance |
3M HDT Heat Shrink Tubing 3M Heat Shrink Tubing HDT is a designed to provide reliable performance as well as excellent mechanical and environmental protection. This flame-retardant product combines the important advantage of.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M SJ6100 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4004 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4008 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4026 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4056 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4085 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Solvent Resistance |
3M MDT Tubing 3M MDT Tubing offers increased flexibility in combination with excellent abrasion, corrosion and environmental resistance properties and meets MIL-DTL-23053/15, Class 2. Uncoated product (without se.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D149 |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Short Term |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |