Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D-149 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.015" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Dielectric Strength | 59.0 kV/mm | 1500 kV/in | |
Von Roll Isola IMI MICA MAT® Inorganic Bonded Mica Plate Data provided by Von Roll Isola USA.Rigid plate designed for use as a non-conducting structural component up to 760°C. 100% inorganic so it maintains good physical and electrical properties at ele.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | |
Tra-Con Tra-Bond Ablebond 933-1.5 Moisture Resistant Encapsulant TRA-BOND 933-1.5 electrically insulating epoxy encapsulant is formulated to provide a smooth crown over the device of wire bonds. This encapsulant provides protection from thermal and mechanical sho.. |
|||
Dielectric Strength | 59.0 kV/mm | 1500 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D149 |
ExxonMobil LDPE LD 157CW Wire & Cable Low Density Polyethylene Resin Product Description: LD 157CW is a medium density LDPE recommended for the production of Low Voltage power cable insulation, using the on-step silane cross0linking technology. The grade contains a h.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil LLDPE LL 6101RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil LLDPE LL 6101XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D149 |
ExxonMobil LLDPE LL 6201RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D149 |
ExxonMobil LLDPE LL 6201XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil LLDPE LL 6301RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil LLDPE LL 6301XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D149 |
Arlon 514B12R006 0.006" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2116 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | 30% RH |
3M Novec™ 2702 Electronic Grade Coating 3M™ Novec™ 2702 Electronic Grade Coating is designed for protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 2 wt% fluorochemical polymer coa.. |
|||
Dielectric Strength | >= 59.1 kV/mm @Thickness 0.0508 mm |
>= 1500 kV/in @Thickness 0.00200 in |
Cured; ASTM D149 |
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e.. |
|||
Dielectric Strength | >= 59.1 kV/mm @Thickness 0.0762 mm |
>= 1500 kV/in @Thickness 0.00300 in |
Cured; ASTM D149 |
Aptek 7503LM-PMF UV Urethane Conformal Coating UV-cured, low modulus, shadow cures under components. Excellent adhesion without primer. Repairable. Qualified to MIL-I-46058C, types UR and AR. Castable version – UVIKOTE 7504 LM-PMF.Information p.. |
|||
Dielectric Strength | >= 59.1 kV/mm @Thickness 0.0762 mm |
>= 1500 kV/in @Thickness 0.00300 in |
Cured; ASTM D149 |
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.Information provided by Aptek Laboratories, .. |
|||
Dielectric Strength | >= 59.1 kV/mm @Thickness 0.0762 mm |
>= 1500 kV/in @Thickness 0.00300 in |
Cured; ASTM D149 |
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic component.. |
|||
Dielectric Strength | >= 59.1 kV/mm @Thickness 0.0762 mm |
>= 1500 kV/in @Thickness 0.00300 in |
Cured; ASTM D149 |
Aptek UVISTAKE 7206 UV Curing, Urethane staking compound UVISTAKE 7206 is a 100% solid, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mount.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D149 |
3M 7945MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D149 |
3M 9061MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Dielectric Strength | >= 59.1 kV/mm @Thickness 0.0762 mm |
>= 1500 kV/in @Thickness 0.00300 in |
Cured; ASTM D149 |
Aptek 2503-A/B Low modulus urethane conformal coating APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | ASTM D149 |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Dielectric Strength | 59.1 kV/mm | 1500 kV/in | IPC TM-650 2.5.6.2 |
Arlon 45N Multifunctional Epoxy Laminate and Prepreg Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi.. |
|||
Dielectric Strength | 59.0 kV/mm @Temperature 23.0 °C |
1500 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |