Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 5.91 kV/mm @Thickness 3.17 mm |
150 kV/in @Thickness 0.125 in |
Condition - A Step/Step |
Industrial Laminates/Norplex MC603 Paper Base Laminate
(discontinued **) Description: MC603 is constructed from electrical grade of kraft paper and a specially modified phenolic resin system, and is designed to be used in tap changers, coil support plates and terminal pa.. |
|||
Dielectric Strength | 5.91 kV/mm | 150 kV/in | |
Saint-Gobain CHR® M751 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Strength | 5.90 kV/mm | 150 kV/in | ST; ASTM D149 |
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Dielectric Strength | 5.91 kV/mm | 150 kV/in | ASTM D149 |
Devcon Underwater Repair Putty (UW) Epoxy Emergency Repair ProductsComments: High-performance technology for repairing, patching and rebuilding equipment in habitually wet environments, even under water. Eliminates the need for substrate t.. |
|||
Dielectric Strength | 5.91 kV/mm | 150 kV/in | |
Dow Corning SE 4446 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility.Information provided by Dow Corning |
|||
Dielectric Strength | 5.91 kV/mm | 150 kV/in | |
Aremco AREMCOLOX™ 502-676 Machinable Magnesium Oxide Full-fired, fine grain, high purity MgO ceramic. Inert to molten metals, slags, superconductors. Broad line of standard crucibles. Custom parts made to print. |
|||
Dielectric Strength | 5.91 kV/mm | 150 kV/in | |
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Dielectric Strength | 5.91 kV/mm | 150 kV/in | |
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina Fine grain castable for potting and producing small tools. |
|||
Dielectric Strength | 5.91 kV/mm | 150 kV/in | |
Aremco Ceramacast™ 576-N High Temperature Potting & Casting Alumina Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devic.. |
|||
Dielectric Strength | 5.90 kV/mm | 150 kV/in | |
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils .. |