Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 510 kV/mm @Temperature 23.0 °C |
13000 kV/in @Temperature 73.4 °F |
DC; DIN 40634 or VDE 0345 in air |
Mitsubishi Hostaphan® RN, 36 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |