Polymer Property : Dielectric Strength = 1220 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength >= 48.0 kV/mm

@Temperature 200 °C
>= 1220 kV/in

@Temperature 392 °F
50 Hz; Average is > 80 kV/mm
Professional Plastics Kaptrex® Polyimide Film
Kaptrex polyimide film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. Kaptrex film provides excellent electrical proper..
Dielectric Strength 48.0 kV/mm
1220 kV/in
IEC 243
LG Chemical HI-121 ABS, High Impact
Feature: Injection Molding, Well Balanced Mechanical PropertiesApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information Provided by LG Chem
Dielectric Strength 48.0 - 61.8 kV/mm
1220 - 1570 kV/in
ASTM D149
Zeus THV Tubing
THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity.
Dielectric Strength 48.0 kV/mm
1220 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Hippe PTFE
Good chemical resistance. High thermal stability. Flame resistance. Lowest coefficient of friction among all solid plastics. Very good dielectric properties. Very high weathering resistance.Info..
Dielectric Strength 48.0 kV/mm
1220 kV/in
DIN 53481/VDE 0303
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Dielectric Strength 48.0 - 272 kV/mm

@Temperature 200 - 200 °C
1220 - 6910 kV/in

@Temperature 392 - 392 °F
Average value: 157 kV/mm Grade Count:3
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..