Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 4.80 kV/mm | 122 kV/in | Step by Step; ASTM D149 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Dielectric Strength | 4.80 kV/mm | 122 kV/in | ASTM D149 |
Tipco Tipcolite® TG 618 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Dielectric Strength | 4.80 - 30.0 kV/mm | 122 - 762 kV/in | Average value: 12.3 kV/mm Grade Count:21 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |
|||
Dielectric Strength | 4.80 kV/mm | 122 kV/in | 60 Hz, wet, SS; ASTM D149 |
Sumitomo Bakelite North America FM 1132P Cellulose Reinforced Phenolic Novolac FM 1132P is a two-stage phenolic molding compound reinforced with cellulose in pellet form. FM-1132P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-10. (Replaces Militar.. |