Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 46.0 kV/mm @Thickness 1.00 mm |
1170 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East) NORYL NH5110E is a flame retardant, non halogenated, impact modified extrusion grade. Developed for low beard-growth, with a Vicat B/120 of 138 Deg C, according to ISO 306 and a UL-94 rating of V1@ .. |
|||
Dielectric Strength | 46.0 kV/mm | 1170 kV/in | IEC 60243-1 3 |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Dielectric Strength | 46.0 kV/mm | 1170 kV/in | Breakdown |
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL) |
|||
Dielectric Strength | 46.0 kV/mm | 1170 kV/in | DIN 53481/VDE 0303 |
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Dielectric Strength | 46.0 kV/mm | 1170 kV/in | IEC 243 |
LG Chemical HF-380 ABS, High Flow, High Impact Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem |