Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.7 - 43.0 kV/mm | 450 - 1090 kV/in | Average value: 27.4 kV/mm Grade Count:22 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Dielectric Strength | 19.0 - 43.0 kV/mm | 483 - 1090 kV/in | Average value: 25.5 kV/mm Grade Count:8 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Strength | 19.7 - 43.0 kV/mm | 500 - 1090 kV/in | Average value: 31.2 kV/mm Grade Count:24 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Strength | 17.7 - 43.0 kV/mm | 450 - 1090 kV/in | Average value: 28.8 kV/mm Grade Count:50 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 19.7 - 43.0 kV/mm | 500 - 1090 kV/in | Average value: 33.0 kV/mm Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Dielectric Strength | 24.0 - 43.0 kV/mm | 610 - 1090 kV/in | Average value: 41.1 kV/mm Grade Count:11 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |