Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.0 - 39.0 kV/mm | 864 - 991 kV/in | Average value: 36.2 kV/mm Grade Count:5 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Dielectric Strength | 1.10 - 39.0 kV/mm | 27.9 - 991 kV/in | Average value: 26.4 kV/mm Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |