Polymer Property : Dielectric Strength = 30.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 11.8 - 30.5 kV/mm
300 - 775 kV/in
Average value: 22.6 kV/mm Grade Count:8
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Dielectric Strength 9.00 - 30.5 kV/mm
229 - 775 kV/in
Average value: 28.2 kV/mm Grade Count:11
Overview of materials for Nylon 11, Powder
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate M..