Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.40 - 16.7 kV/mm | 188 - 424 kV/in | Average value: 12.6 kV/mm Grade Count:12 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
Dielectric Strength | 8.50 - 16.7 kV/mm | 216 - 424 kV/in | Average value: 12.0 kV/mm Grade Count:30 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Strength | 14.8 - 16.7 kV/mm | 375 - 425 kV/in | Short Time |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Dielectric Strength | 14.8 - 16.7 kV/mm | 375 - 425 kV/in | short time |
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic.. |
|||
Dielectric Strength | 14.8 - 16.7 kV/mm | 375 - 425 kV/in | Short Time |
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications.. |
|||
Dielectric Strength | 15.2 - 16.7 kV/mm | 386 - 424 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 99 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |