Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.8 - 14.7 kV/mm | 274 - 373 kV/in | Average value: 12.5 kV/mm Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |