Electrical Properties Metric English Comments
Dielectric Strength 0.984 - 1.38 kV/mm
25.0 - 35.0 kV/in
IEC 60243-1
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
Dielectric Strength 0.984 - 1.38 kV/mm
25.0 - 35.0 kV/in
IEC 60243-1
Raschig Group SURAPLAST 54 UPA
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..