Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 94.5 kV/mm | 2400 kV/in | |
Saint-Gobain CHR® 2255-6 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Strength | 94.5 kV/mm | 2400 kV/in | 5 mil film; ASTM D149 |
3M Dyneon™ FEP 6322Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6322Z was designed primarily for high-speed extrusion for wire insulation. Its distinguishing features include:High extrusion speedHigh thermal stabilityWide processing windowSuperior ele.. |
|||
Dielectric Strength | 94.5 kV/mm | 2400 kV/in | |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |