Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.10 kV/mm | 206 kV/in | AC 60 Hz; 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 8.10 kV/mm | 206 kV/in | Short Time; ASTM D149 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |