Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.00 kV/mm | 203 kV/in | |
Pyrotek TS-101 Thermoset Electrical Insulation Product (Nema Grade: C) Cotton reinforcement, Phenolic resin, Natural color. High Impact strength. Good machining qualities.Information provided by Pyrotek. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | ASTM D149 |
Parker Chomerics THERM-A-GAP™ GEL 30 High Performance Fully Cured Dispensable Gel Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl.. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | ASTM D149 |
Parker Chomerics THERM-A-GAP™ GEL 8010 High Performance Fully Cured Dispensable Gel Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl.. |
|||
Dielectric Strength | 8.00 - 14.2 kV/mm | 203 - 361 kV/in | Average value: 11.2 kV/mm Grade Count:9 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | Short Time; ASTM D149 |
Plenco 7527 Phenolic, Nodular, Injection Molded
(discontinued **) Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | AC 60 Hz; 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 45Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | |
GBC Cerasilâ„¢ 223U Ceramic Has a lower CTE, better thermal shock resistance, lower firing temperature, and lower consistent shrinkage than steatite.Applications: ideal for volume production of small pressed insulators often r.. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | Perpendicular, Short-term, in air; ASTM D149 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | Short Time; ASTM D149 |
Plenco 7507 Phenolic, Granular, Injection Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | ASTM D149 |
Tipco Tipcolite® TX 312 Phenolic Compound, Wood Flour & Minerals having Soft Flow & Lower Density Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Dielectric Strength | 8.00 kV/mm @Thickness 3.00 mm |
203 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Mechanical and electrical applications. High mechanical strength. Self-extinguishing, halogen-free. Good resistance to chemicals.Information provided by Elektro-Isola |
|||
Dielectric Strength | 8.00 - 10.5 kV/mm @Temperature 90.0 °C |
203 - 267 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Dielectric Strength | >= 8.00 kV/mm @Temperature 90.0 °C |
>= 203 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en.. |
|||
Dielectric Strength | 8.00 - 10.0 kV/mm @Temperature 90.0 °C |
203 - 254 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | DIN 53752 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Dielectric Strength | 8.00 - 10.5 kV/mm @Temperature 90.0 °C |
203 - 267 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Dielectric Strength | >= 8.00 kV/mm @Temperature 90.0 °C |
>= 203 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 157 Phenolic Molding Long glass fiber Filler, Compression Molded Characteristics:Shock resistant ( High impact strength )Very good mechanical strengthGood dielectric strengthLow water absorptionLow shrinkageColor-pale brown, black, dark brown, green etc.Medium/st.. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | |
Pyrotek TS-81 Thermoset Electrical Insulation Product (Nema Grade: CE) Cotton reinforcement, Phenolic resin, Natural / Tan color. Economy grade. Good acid resistance.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulat.. |
|||
Dielectric Strength | 8.00 - 38.0 kV/mm | 203 - 965 kV/in | Average value: 23.8 kV/mm Grade Count:27 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Dielectric Strength | 8.00 kV/mm | 203 kV/in | 60 Hz, wet, SS; ASTM D149 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |