Polymer Property : Dielectric Strength = 7.44 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 7.44 - 60.0 kV/mm
189 - 1520 kV/in
Average value: 24.6 kV/mm Grade Count:21
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Dielectric Strength 7.44 - 24.0 kV/mm
189 - 610 kV/in
ASTM D149
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..