Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir R 540E Polystyrene HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection
moldings. Designation: Thermoplastics IS.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir RT 461F Polystyrene High impact, heat resistant polystyrene with good stiffness. Recommended for improving the thermal performance of injection moulded technical parts which are submitted to high temperature in service.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR Very high environmental stress cracking resistant (VH ESCR) HIPS.ICE S 900 exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents, and in particular to cyclopent.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-23 UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal pr.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR PD RR745E High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,088-03-07-12 Environmental stress cracking resistant (ESCR) HIPS. It combines high impact strength with high chemical r.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR RC3 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-18 Special high impact, high gloss polystyrene grade. Suitable for injection molding in the appliances sector.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-03-04-23 UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded high impact polystyrene with excellent light .. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® S 131 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | 200µm film; IEC 60243-1 |
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60250 |
Polyram PlusTek PB318G9 Nylon 6 for Injection Molding, 45% Glass-fiber Reinforced, UV Stabilized 45% Glass-fiber reinforced Nylon 6, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | VDE 0303/4 |
Polyram PlusTek PB320G3 Nylon 6, 15% Glass Fiber, Flame Retardant 15% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® F2 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR SRL550 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,E,083-12-07-18 High impact, easy flow polystyrene with good elasticity at low temperatures. Used for sheet extrusion and .. |
|||
Dielectric Strength | 65.0 - 146 kV/mm | 1650 - 3710 kV/in | Average value: 75.1 kV/mm Grade Count:8 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |