Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 6.20 - 17.4 kV/mm | 157 - 442 kV/in | Average value: 11.6 kV/mm Grade Count:21 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Dielectric Strength | 6.20 kV/mm | 157 kV/in | Step by Step; ASTM D149 |
Plenco 00732 Melamine-Phenolic, Granular, Injection Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Dielectric Strength | 6.20 kV/mm | 157 kV/in | Step by Step; ASTM D149 |
Plenco 3303 Phenolic, Granular, Injection Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |