Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 5.71 kV/mm | 145 kV/in | |
Saint-Gobain COHRlastic® R10450 Medium Fiberglass Reinforced Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Dielectric Strength | 5.71 kV/mm | 145 kV/in | |
Saint-Gobain COHRlastic® R10460 Medium Flame Retardant Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Dielectric Strength | 5.71 kV/mm | 145 kV/in | |
Saint-Gobain COHRlastic® R10470 Firm General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Dielectric Strength | 5.71 kV/mm | 145 kV/in | |
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Dielectric Strength | 5.71 kV/mm | 145 kV/in | |
Saint-Gobain COHRlastic® R10480 Medium Low Compression Set Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Dielectric Strength | 5.71 kV/mm | 145 kV/in | |
Saint-Gobain COHRlastic® R10480 Soft Low Compression Set Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Dielectric Strength | 5.71 kV/mm | 145 kV/in | |
Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R1.. |