Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 49.0 kV/mm @Thickness 3.20 mm |
1240 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Dielectric Strength | 49.0 kV/mm @Thickness 3.20 mm |
1240 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Dielectric Strength | 49.0 kV/mm @Thickness 3.20 mm |
1240 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Dielectric Strength | 49.0 kV/mm @Thickness 3.20 mm |
1240 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Dielectric Strength | 49.0 kV/mm @Thickness 3.20 mm |
1240 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
Dielectric Strength | 49.0 kV/mm | 1240 kV/in | ASTM D149 |
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Dielectric Strength | 49.0 kV/mm | 1240 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 30 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | >= 49.0 kV/mm | >= 1240 kV/in | DIN 53481/VDE 0303 |
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhi.. |
|||
Dielectric Strength | >= 49.0 kV/mm | >= 1240 kV/in | DIN 53481/VDE 0303 |
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue.. |