Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 42.5 kV/mm | 1080 kV/in | |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |