Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 35.4 kV/mm | 899 kV/in | DIN 53481 |
Polikim ULPOLEN® 1000 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | DIN 53481 |
Polikim ULPOLEN® 500 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | Method A; ASTM D149 |
S&E Specialty Polymers TufShield™ FS-1000H-UVFG Insulating Compound Application: A UV and fungus resistant lead-free, low smoke generating, highly flame retardant jacketing and insulation compound designed for Plenum cable application. Compound exhibits excellent pr.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | ASTM D149 |
Rochling Engineered Plastics Polystone® MPG Glass filled (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | ASTM D149 |
Rochling Engineered Plastics Polystone® Natural (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | ASTM D149 |
Rochling Engineered Plastics Polystone® XL Cross linked (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
Tra-Con Tra-Bond 293-1M General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1M general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper and brass. The 293-se.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s.. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | High Humidity; ASTM D1000 |
3M 1400 Economy Vinyl Electrical Tape 3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chlor.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon R34572R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1080 Style FiberglassAppearance: Red silicone rubber on fiberglass clothThis data represents typical value.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon R37053W007 0.007" (0.178 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1 Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 2133 FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneThis data represents ty.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon 48B12R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be used.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
3M Scotch® FP-301VW Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301VW has the same outstanding balance of electrical, physical and chemical properties as FP-301 tubing, and is specially engineered for excellent flame resistance. FP.. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | ASTM D149-95 |
Multibase Multi-ABS 2925 FR Flame Retardant ABS Data provided by Multibase. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
3M MW Heat Shrink Tubing 3M Heat Shrink Tubing MW is a semi-rigid, 110°C heat-shrinkable polyolefin tubing that is a co-extruded and selectively cross-linked to provide an integral, meltable inner wall. When heated in exce.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive
(discontinued **) Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | ASTM D149-95 |
Multibase Multi-ABS 3075 High Impact Data provided by Multibase. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be us.. |
|||
Dielectric Strength | 35.4 kV/mm | 899 kV/in | ASTM D149 |
Rochling Engineered Plastics Polystone® Reprocessed (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |