Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 32.0 kV/mm | 813 kV/in | |
Polimeri Europa SINKRAL PD H210/K ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,085-25-16-25 Flame retarded (PBBE free) injection moulding grade, rated UL94-5V at 3.2 mm thick and UL 94V-0 at.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243 |
Solvay TECHNYL® A 238 Black 21 N PA66, Conditioned Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | |
Styrolution NOVODUR® P2HGV ABS, 16% Glass Fiber Injection molding grade, glass reinforced (16%).Applications: Automotive industry: instrument panels, rear light housings, internal components of domestic appliances. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60250 |
Polyram PlusTek PA801 Nylon 6.6 Copolymer for Injection Molding, Impact Modified Impact modified Nylon 6.6 copolymer for injection molding application.Information provided by Polyram. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40 Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BGZ-15 PA6-GF15 Information provided by EMS Grivory |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 16 GM nat PA12 Grilamd L16 GM is a low-viscosity, non-reinforced PA 12 grade, UV- and heat-stabilized. The modification with a crystallization regulator causes a quick freeze and a fine, crystalline structure. Due.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 20 G PA12 Product Description: Grilamid L 20 LG is a normal viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics Low moisture absorpt.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 20 L PA12 Product Description: Grilamid L 20 L is a medium viscosity Polyamide 12 (PA12) extrusion type. It is UV and heat stabilized. Its main features are: High surface quality Very good UV and heat resista.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 nat 6112 PA12 Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples:.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 40 X PA12-I Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40 Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4164 black 9225 PA*-GF30 Product description: Grivory XE 4164 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | ASTM D149, IEC 243 |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 20 X PA12-I Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | 50%RH; IEC 60243-1 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 32.0 - 35.0 kV/mm | 813 - 889 kV/in | Average value: 33.7 kV/mm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |