Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 31.0 kV/mm | 787 kV/in | STN IEC 60243 |
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Dielectric Strength | 31.0 - 49.0 kV/mm | 787 - 1240 kV/in | Average value: 42.7 kV/mm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
Plastcom SLOVASTER® B1 GF 20 000/1 PBT, 20% glass fibre FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticit.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | ASTM D149 |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | |
Ineos ABS Lustran® H604 Standard impact strength.,Property data per ISO test methods. |
|||
Dielectric Strength | 31.0 kV/mm @Thickness 1.00 mm |
787 kV/in @Thickness 0.0394 in |
d.a.m.; IEC 60243-1 |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | IEC 60243-1 |
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Dielectric Strength | 31.0 kV/mm @Thickness 1.00 mm |
787 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant Feature: Injection Molding, sPS+GF30%, Flame RetardantApplication: Pump Units, Pick-up Lends Holder, etcCAS No. 9003-53-6, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® AS V0 PA66 Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® 410 Paper, 24 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BG-50 PA6-GF50 Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TR 55 PA12/MACMI Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties.. |
|||
Dielectric Strength | 31.0 kV/mm | 787 kV/in | ASTM D149 |
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr.. |