Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 29.1 kV/mm | 740 kV/in | ASTM D149 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Dielectric Strength | 29.1 kV/mm | 740 kV/in | ASTM D149 |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Dielectric Strength | 29.1 kV/mm | 740 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Dielectric Strength | 29.1 kV/mm | 740 kV/in | ASTM D149 |
Arlon 51106R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 29.1 kV/mm | 740 kV/in | ASTM D149 |
Arlon 51146R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 29.1 kV/mm | 740 kV/in | ASTM D149 |
Arlon 51276R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 29.1 kV/mm | 739 kV/in | ASTM D149 |
Arlon 51576R015D 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical v.. |