Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 29.0 kV/mm | 737 kV/in | |
Ineos ABS Lustran® QE 1455/L2, Injection Grade
(discontinued **) Injection molding grade, increased heat resistance, medium gloss, UV-stabilized grade.Applications: Automotive: body parts.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)
(Unverified Data**) Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 19 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 24 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® FC 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® FC 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® MX 1000 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | ASTM D149 |
Lavergne VYPET VNT 630 FR PET 30% Glass Reinforced, Flame Retardant Vypet VNT 630 FR is a 30% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | |
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243 |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | VDE 0303/4 |
Polyram RamSter PF320G2 PBT, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | dry; IEC 60243-1 |
DSM Novamid® ST220 NAT PA6-I Impact Modified, Injection Molding, Medium Viscosity |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BS V0 PA6 Product description: Grilon BS V0 is an unreinforced, normal viscosity, self-extinguishing PA6 injection molding grade. Grilon BS V0 has the following important properties: Halogen and phosphorous-f.. |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 400H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | ASTM D149 |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 540V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 540Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 220V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |