Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 272 kV/mm | 6910 kV/in | |
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film 120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme.. |