Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.6 kV/mm | 701 kV/in | DIN 53481 |
Polikim ULPOLEN® 300 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Dielectric Strength | 27.6 kV/mm | 701 kV/in | Short Term; ASTM D149 |
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 27.6 - 100 kV/mm | 701 - 2540 kV/in | Average value: 54.8 kV/mm Grade Count:49 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Dielectric Strength | 27.6 kV/mm @Thickness 1.57 mm |
700 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |
|||
Dielectric Strength | 27.6 kV/mm @Thickness 1.57 mm |
700 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP625 Paper Base Laminate Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611. |
|||
Dielectric Strength | 27.6 kV/mm @Thickness 1.60 mm |
701 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PBT/ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF5 HS BK002 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided b.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D-149 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.062" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF5 IM HS BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifie.. |
|||
Dielectric Strength | 27.6 kV/mm | 701 kV/in | 1" electrode in air; ASTM D149 |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Dielectric Strength | >= 27.6 kV/mm | >= 700 kV/in | At 20 mils; ASTM D3755 |
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
Tra-Con Tra-Bond 931-1 Low Viscosity Encapsulant TRA-BOND 931-1 low viscosity epoxy encapsulant is designed for high reliability applications, where capillary action is desired. This encapsulant provides environmental and mechanical protection.Inf.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | In Oil; ASTM D149 |
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51141R015 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51146R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat.. |
|||
Dielectric Strength | 27.6 kV/mm | 701 kV/in | Arlon SQA-TMS-020 |
Arlon 920-10CxxFR-P1 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, brown, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51106R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass This data represents typical values for the production ma.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
3M EPS-400 Heat Shrink Tubing 3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |