Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Covestro Petlon® 8535 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Impact Modified: Excellent Electrical Properties, High Heat ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temp.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | |
Saint-Gobain CHR® 2915-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Plastics Group Polifil® 628L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Arlon 51576B015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
3M Scotch-Weld™ DP605NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
Arlon 51576W015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: White silicone gum on glass fabricThis data re.. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | 1" electrode in air; ASTM D149 |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |