Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Dielectric Strength | 25.0 - 35.0 kV/mm | 635 - 889 kV/in | IEC 60243-1 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | ISO.243 DIN.53481 |
Omnia Plastica PA6 GF Akulon GF - Dry Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® S223-HG6U (Cond.) 33% Glass Reinforced Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 1.00 mm |
635 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage
(discontinued **)& Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | ASTM D149 |
Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin Flame retardant, BLACKApplications: ConnectorsInformation provided by API-Kolon. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 |
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 |
Global EPP PA 6C WFN Cast Polyamide 6 + Wax Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Dielectric Strength | 25.0 - 85.0 kV/mm | 635 - 2160 kV/in | DIN 53481 |
Isoflon PETP Polyethylene terephthalate Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 2.00 mm |
635 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific) Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | JIS K2111 |
Toyobo PELPRENE™ S1002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 2.00 mm |
635 kV/in @Thickness 0.0787 in |
ASTM D149 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Stanyl® TW341 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Covestro Bayblend® KU 2-1468 Polycarbonate/ABS Blend Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | Conditioned; CEI 60243-1 |
Addiplast Addinyl A2 G30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | DIN 53481 |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | dry; IEC 60243-1 |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | DIN 53481 |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
3M Dyneon™ Fluorel™ FG-5690Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |