Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Conditioned; ASTM D149 |
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6 Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | ASTM D149 |
KKPC Kuhmo GP 125EI General Purpose GPPS Key features: For phonograph, good profile properties. Common Uses: CD-CASE, THIN-WALLGPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding proces.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | ASTM D149 |
KKPC Kuhmo GP 150 High Heat Resistant, High Rigidity GPPS Key features: High Heat-resistance, High Strength Common Uses: Vegetable boxes in refrigerators, humidifiers, lighting apparatus, cassette tape cases, parts of optical instruments, PS paper, etc.GPP.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6/6 GF33 TL10 HS 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PSU CR X Availability: North AmericaForms: PelletsAdditive: TPU Impact Modifier Features: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® HIPS FR V-2 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® HIPS FR-1 Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PBT GF10 CBA 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: FoamableAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | >= 21.7 kV/mm | >= 550 kV/in | ASTM D149 |
Borealis Visico™/Ambicat™ LE4421/LE4476 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4421 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Dielectric Strength | >= 21.7 kV/mm | >= 550 kV/in | ASTM D149 |
Borealis Visico™/Ambicat™ LE4423/LE4472 Black, Fast Curing, Silane Crosslinkable LDPE Compound for Weather Resistant Covering/Insulation of Overhead Cables Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Dielectric Strength | >= 21.7 kV/mm | >= 550 kV/in | ASTM D149 |
Borealis Visico™/Ambicat™ ME4425/LE4476 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4476, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Dielectric Strength | >= 21.7 kV/mm | >= 550 kV/in | ASTM D149 |
Borealis Visico™ ME4425/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico ME4425/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. ME4425 is a medium-density ethylene vin.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Test run on 1/8" specimens. |
Loctite® Durabond® E-214HP Epoxy Adhesive Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | ASTM D149 |
Arlon LW201R##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | ASTM D149 |
Arlon 51141R027 0.0270" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values .. |
|||
Dielectric Strength | >= 21.7 kV/mm | >= 550 kV/in | ASTM D149 |
Borealis Visico™/Ambicat™ LE4421/LE4472 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4421 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Dielectric Strength | 21.7 kV/mm | 550 kV/in | ASTM D149-97 |
Saint-Gobain Tygon® Tygoprene® XL-60 Pump Tubing Formulation Designed specifically for use in peristaltic pump applications, Tygoprene® Pump Tubing maintains a pump life of over 500 hours. It is extremely flexible and exhibits superior flex life, reducing do.. |