Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.65 kV/mm | 549.9 kV/in | 1" electrode in air; ASTM D149 |
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s.. |