Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.3 kV/mm @Thickness 3.20 mm |
516 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dielectric Strength | 20.3 kV/mm @Thickness 3.20 mm |
516 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dielectric Strength | 20.3 kV/mm @Thickness 3.20 mm |
516 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Dielectric Strength | 20.3 kV/mm @Thickness 3.20 mm |
516 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Dielectric Strength | 20.3 kV/mm @Thickness 1.91 mm |
516 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials RTV11 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Dielectric Strength | 20.3 kV/mm @Thickness 1.90 mm |
516 kV/in @Thickness 0.0748 in |
|
Momentive Performance Materials RTV41 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Dielectric Strength | 20.3 kV/mm @Thickness 1.91 mm |
516 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Dielectric Strength | 20.3 kV/mm @Thickness 3.20 mm |
516 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |