Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 2.90 kV/mm | 73.7 kV/in | |
Pyrotek NAD-11 Structural Insulation Board NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation .. |
|||
Dielectric Strength | 2.90 kV/mm | 73.7 kV/in | |
Pyrotek NAD-500 Electrical Insulation Product Cement reinforcement, Inorganic fiber resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasket.. |