Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-50-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-60-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | |
Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C). |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | Perpendicular S/T in Air; ASTM D-149 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
Dielectric Strength | 2.00 kV/mm @Diameter >=3.00 mm |
50.8 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments.. |
|||
Dielectric Strength | 2.00 kV/mm @Thickness 3.00 mm |
50.8 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Impact-resistant, noise-reducing and wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environ.. |
|||
Dielectric Strength | 2.00 kV/mm @Diameter >=3.00 mm |
50.8 kV/in @Diameter >=0.118 in |
96hr/105°C+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronit B 66 Phenolic, Paper Reinforcement, Dark Brown, Tubes Description: Specially designed for high-voltage insulation with high requirements for insulating capacity along the tube.Applications: Insulating tubes in high-voltage switchgear and tap changers.... |
|||
Dielectric Strength | 2.00 kV/mm @Diameter >=3.00 mm |
50.8 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Mechanical and electrical applications. High mechanical strength. Self-extinguishing, halogen-free. Good resistance to chemicals.Information provided by Elektro-Isola |
|||
Dielectric Strength | 2.00 kV/mm @Diameter >=3.00 mm |
50.8 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP FR Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relati.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | Perpendicular S/T in Air; ASTM D-149 |
Glastic GLASTHERM HT Insulation Sheet Glastherm Grade HT is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT is completely as.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Dielectric Strength | 2.00 kV/mm | 50.8 kV/in | ASTM D149 |