Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.1 kV/mm | 485 kV/in | ASTM D149 |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Dielectric Strength | 19.1 kV/mm @Thickness 3.20 mm |
485 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® HR426 PBT AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
Dielectric Strength | 19.1 kV/mm @Thickness 3.20 mm |
485 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® HR426 PBT (Asia Pacific) AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
Dielectric Strength | 19.1 kV/mm | 485 kV/in | |
Dow Corning 3-4133 DIELECTRIC GEL KIT Two-part, clear, heat cure, and firm.Information provided by Dow Corning |
|||
Dielectric Strength | >= 19.1 kV/mm | >= 486 kV/in | ASTM D149 |
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as .. |
|||
Dielectric Strength | 19.1 kV/mm | 485 kV/in | ASTM D149 |
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic.. |
|||
Dielectric Strength | 19.1 kV/mm | 485 kV/in | ASTM D149 |
Arlon 55146R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sili.. |
|||
Dielectric Strength | 19.1 kV/mm | 486 kV/in | Short Time |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Dielectric Strength | 19.1 kV/mm | 486 kV/in | ASTM D149 |
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value.. |
|||
Dielectric Strength | 19.1 kV/mm | 485 kV/in | ASTM D149 |
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic.. |
|||
Dielectric Strength | 19.1 kV/mm | 486 kV/in | ASTM D149 |
Arlon R37732W079 0.079" (2.01 mm) Cured Silicone Rubber with Treated FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Treated FEP FilmThis data represents typical values for the production material. The data should not be used to w.. |