Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Dielectric Strength | 17.3 kV/mm | 439 kV/in | |
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF30 IM HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/10 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/10 GF50 L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6,6 IM 3757 Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.20 mm |
439 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: UV Stabilizer, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Good UV.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF43 IM HS L 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM1 L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedInformatio.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulat.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo.. |
|||
Dielectric Strength | >= 17.3 kV/mm @Thickness 3.17 mm |
>= 440 kV/in @Thickness 0.125 in |
|
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Dielectric Strength | 17.3 kV/mm | 439 kV/in | Short Time, 500 V/sec rate-of-rise; ASTM D 149 |
Eastman Eastar AN004 Natural PCTA Copolyester EASTAR AN004 Copolyester contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exp.. |
|||
Dielectric Strength | 17.3 kV/mm | 439 kV/in | ASTM D149 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |
|||
Dielectric Strength | 17.3 kV/mm | 439 kV/in | ASTM D149 |
Ashley Polymers Ashlene® 528L-33G Nylon 66, 33% Glass Reinforced General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufactur.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | ASTM D149 |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | ASTM D149 |
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Dielectric Strength | 17.3 kV/mm | 439 kV/in | step-by-step; ASTM D149 |
Ascend Performance Materials VYDYNE® R533 Nylon, 33% Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |