Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 160 kV/mm @Thickness 3.00 mm |
4060 kV/in @Thickness 0.118 in |
ASTM D149 |
Solvay Specialty Polymers Ajedium™ Film Thermoplastic Polyimide (PI, TP) TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior ra.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 815 High Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 815 is a high heat resistant, high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stab.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 818 Easy Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which r.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 822 Standard Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 822 is a good flow, environmentally friendly high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good d.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 849 High Flow, High Heat Resistance Polystyrene Total Petrochemicals Polystyrene 849 is a high flow, high heat resistant polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stabil.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 850S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 850S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 855S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 855S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 856S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 863 High Flow Flame Retardant Deca Polystyrene Total Petrochemicals Polystyrene 863 is a high flow, heat resistant, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensiona.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | ASTM D149 |
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi.. |
|||
Dielectric Strength | 160 kV/mm | 4060 kV/in | at 0.075 mm |
Goodfellow Polyethylene Naphthalate (PEN) Film A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colo.. |
|||
Dielectric Strength | >= 160 kV/mm | >= 4060 kV/in | |
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Dielectric Strength | >= 160 kV/mm | >= 4060 kV/in | ASTM D149 |
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |