Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 140 kV/mm | 3560 kV/in | K20/P50; IEC 60243-1 |
Styrolution Styrolux® 656 C SBC Description: Styrolux® 656 C is a clear styrene-butadiene copolymer (SBC) with enhanced flow properties. It is used almost exclusively for injection molding of rigid, tough parts requiring highes.. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | K20/P50; IEC 60243-1 |
Styrolution Styrolux® 684 D SBC Description: Styrolux® 684 D is a clear styrene-butadiene copolymer (SBC) used in injection molding for parts with enhanced toughness as well as in sheet and film extrusion and blow molding. Part.. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1101 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1101 P Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1101 R Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2340 P Polypropylene Grade with nucleating agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2348 TC Polypropylene Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2448 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2500 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2900 H Polypropylene Injection molded and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 3200 MC Polypropylene Cast film without slip and blocking agents.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 3225 MC Polypropylene Grade containing slip and blocking agents, for cast film with medium slip.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 3236 MC Polypropylene Grade containing slip, blocking and antistatic agents, for cast film with medium slip.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 3325 MC Polypropylene Grade containing slip and blocking agents, for cast film.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm @Thickness 0.100 mm |
3560 kV/in @Thickness 0.00394 in |
ASTM D149 |
3M Dyneon™ ET 6210AZ Fluoroplastic Agglomerate 3M™ Dyneon™ Fluoroplastic Agglomerate ET 6210AZ is a melt processable fluoroplastic consisting mainly of alternating tetrafluoroethylene and ethylene monomer units (ETFE). This partially crystalli.. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1102 J Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1104 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1125 N Polypropylene Cast film with medium slip.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1126 N Polypropylene Grade with slip and antiblocking agents, for cast and water-cooled blown film with very good slip and especially low tendency to block.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 1148 TC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | |
BASF Novolen® 2240 P Polypropylene Nucleated grade for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | IEC 243/1 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Dielectric Strength | 140 kV/mm | 3560 kV/in | IEC 243/1 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |