Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.3 kV/mm | 362 kV/in | Short Term; ASTM D149 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Dielectric Strength | 14.3 kV/mm @Temperature 121 °C, Time 10800 sec |
362 kV/in @Temperature 250 °F, Time 3.00 hour |
0.0625 in. thickness; ASTM D149 |
Garlock GYLON® 3500 PTFE Gasketing, Silica Filler PTFE with silica filler.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcellent bolt torque r.. |
|||
Dielectric Strength | 14.3 kV/mm | 363 kV/in | Short Time; ASTM D149 |
Plenco 2535 Phenolic, Granular, Compression Molded PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c.. |
|||
Dielectric Strength | 14.3 kV/mm | 363 kV/in | Short Time; ASTM D149 |
Plenco 2571 Phenolic, Granular, Compression Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Dielectric Strength | 14.3 kV/mm | 363 kV/in | ASTM D149 |
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Dielectric Strength | 14.3 - 15.4 kV/mm | 363 - 392 kV/in | Average value: 15.0 kV/mm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |
|||
Dielectric Strength | 14.3 kV/mm | 363 kV/in | Short Time; ASTM D149 |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
Dielectric Strength | 14.3 - 16.3 kV/mm | 363 - 413 kV/in | short time |
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili.. |