Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Plastcom SLOVAMID 6 GF 10 FRA 5 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 10% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm |
356 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
356 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 1.00 mm |
356 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Dielectric Strength | 14.0 - 111 kV/mm | 356 - 2820 kV/in | Average value: 50.0 kV/mm Grade Count:55 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 85H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 150°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-b Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Dielectric Strength | 14.0 - 26.0 kV/mm | 356 - 660 kV/in | DIN 53481 |
Isoflon PUR Polyurethane Very high wear resistanceHighly resilientInformation provided by Isoflon. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.20 mm |
356 kV/in @Thickness 0.126 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | ASTM D149 |
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h.. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.18 mm |
356 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | GB/T1408.1-2006 |
Sichuan Deyang Haton® hMR61 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics D45 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Dow Corning CY 52-276 KIT Two-part, clear, 1:1, addition cure, low temperature cure, low viscosity, controlled volatility.Information provided by Dow Corning |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 2.8 kV minimum |
Arlon 0.008" (0.2032 mm) Primerless Thermabond® Uncured Silicone (99990A008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 2.8 kV minimum |
Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | 2.8 kV minimum |
Arlon 0.015" (0.381 mm) Primerless Thermabond® Uncured Silicone (99990A015) 0.015 in., ±0.001 (0.38 mm, ±0.038) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.015 in ±0.001(0.38 mm ± 0.038).. |
|||
Dielectric Strength | 14.0 kV/mm @Thickness 3.00 mm |
356 kV/in @Thickness 0.118 in |
ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, Step by Step |
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | |
Elastomer Engineering Elastamide 400 Elastomer Modified RIM Nylon 6 18% crystallinity. Information supplied by Elastomer Engineering. |
|||
Dielectric Strength | 14.0 kV/mm | 356 kV/in | ASTM D149 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |