Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 120 kV/mm | 3050 kV/in | ISO.243 DIN.53481 |
Omnia Plastica PVDF Kynar PVDF is a relatively new fluoropolymer. Like the other fluoropolymers, its best feature is its chemical resistance. The mechanical features of PVDF are notably higher than PTFE and it does not suffe.. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A700 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 120 kV/mm @Thickness 0.100 mm |
3050 kV/in @Thickness 0.00394 in |
ASTM D149 |
Victrex® APTIV® 2000-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous APTIV PEEK 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK .. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | K20/P50; IEC 60243-1 |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek PA103 Nylon 6.6, Injection Molding Polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60250 |
Polyram PlusTek PA106 Nylon 66 for Injection Molding, with Molybdenum Disulfide Nylon 66 with molybdenum disulfide, low friction and high abrasion resistance, for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60250 |
Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding Good surface finish Nylon 6/6.6 alloy for injection molding.Information provided by Polyram. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek PA124 Nylon 6.6, Injection Molding A fast cycle polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek PA600 Nylon 6.6, Heat Stabilized Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek PA602 Nylon 6.6, Heat Stabilized Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek PA604 Nylon 6.6, Heat Stabilized High heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60250 |
Polyram PlusTek PA700BL10 Nylon 6.6 for Injection Molding, UV Stabilized UV Stabilized Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek PA810 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek RA601 Nylon 6.6, Heat Resistant Heat resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60250 |
Polyram PlusTek RA702 Nylon 66 for Injection Molding, UV Stabilized UV stabilized Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 120 kV/mm @Thickness 0.0762 mm |
3050 kV/in @Thickness 0.00300 in |
ASTM D149 |
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat.. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 243; DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek PA100 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek RA102 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60250 |
Polyram PlusTek RA115 Nylon 66 for Injection Molding Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | VDE 0303/4 |
Polyram PlusTek RA116 Nylon 6.6, Injection Molding polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | ASTM D149 |
Asahi Glass F-Clean® Film for Greenhouses F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High ten.. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | ASTM D149 |
Asahi Glass Fluon® ETFE A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Dielectric Strength | 120 kV/mm | 3050 kV/in | ASTM D149 |
Asahi Glass Fluon® ETFE Film Applications: Electronics, Energy Saving, Wallpaper, Sound Suppression Walls, Aviation and SpaceInformation provided by Asahi Glass Company, Inc. |
|||
Dielectric Strength | >= 120 kV/mm | >= 3050 kV/in | ASTM D149 |
CEN® Electronic Material CV Polyimide Film, 6 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Dielectric Strength | >= 120 kV/mm | >= 3050 kV/in | |
CEN® Electronic Material CN Polyimide Film, 6 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |