Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 110 kV/mm | 2800 kV/in | |
Saint-Gobain CHR® K102 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Strength | 110 kV/mm | 2800 kV/in | |
Saint-Gobain CHR® K103 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Strength | 110 kV/mm | 2800 kV/in | ASTM D-149 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.003" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Dielectric Strength | 110 - 130 kV/mm | 2790 - 3300 kV/in | Oil, 0.125mm Thk Tape; ASTM D149 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Dielectric Strength | 110 - 130 kV/mm | 2790 - 3300 kV/in | Oil, 0.125mm Thk Tape; ASTM D149 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Dielectric Strength | 110 kV/mm | 2790 kV/in | ASTM D149, IEC 243 |
EPICHEM Epinyl PA 66 Polyamide 66 |
|||
Dielectric Strength | 110 kV/mm | 2790 kV/in | ASTM D149, IEC 243 |
EPICHEM PA 66 Polyamide 66 |
|||
Dielectric Strength | >= 110 kV/mm | >= 2790 kV/in | |
CEN® Electronic Material CN Polyimide Film, 7 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Dielectric Strength | >= 110 kV/mm | >= 2790 kV/in | ASTM D149 |
CEN® Electronic Material CV Polyimide Film, 7 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |