Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.8 - 90.0 kV/mm | 300 - 2290 kV/in | Average value: 27.8 kV/mm Grade Count:50 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Strength | 11.8 - 90.0 kV/mm | 300 - 2290 kV/in | Average value: 24.1 kV/mm Grade Count:46 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Plenco 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 506 is a two-stage, mineral-filled ph.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
IDI Composites 44-10 HGM Thermoset Polyester, Molding Same as 44-10 HG with Mil Spec MAI-60.Data provided by the manufacturer. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
IDI Composites W-103 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HDPE E GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HDPE GF15 BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PEEK 150 Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PEEK 450 BK Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Compression Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | |
Trelleborg Emerson & Cuming Stycast® E-1000 One-Component Epoxy Low Stress Encapsulant Emerson & Cuming E-1000 Stycast® One-Component Epoxy Low Stress EncapsulantDesigned for the encapsulation of a wide range of stress sensitive electronics. They offer excellent performance at low te.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | ASTM D149 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D1000 |
3M Scotch™ 2200 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Dielectric Strength | 11.8 - 13.0 kV/mm | 300 - 330 kV/in | Short Time |
Bulk Molding Compounds BMC 605LWR Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LWR is a mineral filled, glass fiber reinforced polyester bulk molding compound suitable for compression, transfer and stuffer injection molding. It is designed to provide improved wear resis.. |
|||
Dielectric Strength | 11.8 - 15.7 kV/mm | 300 - 400 kV/in | |
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | Average value: 15.3 kV/mm Grade Count:38 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Dielectric Strength | 11.8 - 18.7 kV/mm | 300 - 475 kV/in | Average value: 15.3 kV/mm Grade Count:5 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 11.8 kV/mm | 300 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional sta.. |
|||
Dielectric Strength | 11.8 - 100 kV/mm | 300 - 2540 kV/in | Average value: 26.8 kV/mm Grade Count:105 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |