Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.0 kV/mm | 279 kV/in | ISO.243 DIN.53481 |
Omnia Plastica PTFE Polytetrafluoroethylene A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond F202 Anaerobic Retainer The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HH190 Anaerobic Gasketmaker Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HM161 Anaerobic Retaining Compound Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HM162 Anaerobic Retainer Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HM163 Anaerobic Retainer Permabond® HM163 is a medium viscosity, thixotropic anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It has been specifically formulated to provide a .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond MH196 Anaerobic Gasketmaker Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond MH199 Anaerobic Gasketmaker Permabond® MH199 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |
|||
Dielectric Strength | 11.0 - 27.0 kV/mm | 279 - 686 kV/in | Average value: 18.1 kV/mm Grade Count:44 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Dielectric Strength | 11.0 - 70.0 kV/mm | 280 - 1780 kV/in | Average value: 27.9 kV/mm Grade Count:55 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 30Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 45T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.17 mm |
280 kV/in @Thickness 0.125 in |
Unconditioned; ASTM D149 |
Garlock Bay State 22 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, smooth rotocured finish. It conforms easily to uneven flange surfaces.Information pr.. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
280 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | Short Time; ASTM D149 |
Plenco 3356 Phenolic, Granular, Injection Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
279 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Dielectric Strength | 11.0 kV/mm | 280 kV/in | ASTM D149 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A011 Anaerobic Threadlocker Permabond® A011 is an anaerobic adhesive designed for locking and sealing threaded or coaxially fitting metal parts where subsequent dismantling is required. Its controlled strength ensures fatigue.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A1044 Anaerobic Threadsealant Permabond® A1044 is a rapid curing sealant designed to lock and seal metal pipe connections, offering very good resistance to even the most aggressive chemicals. Permabond A1044 can be used to seal.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for .. |
|||
Dielectric Strength | 11.0 - 80.0 kV/mm | 280 - 2030 kV/in | Average value: 23.9 kV/mm Grade Count:27 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A1046 Anaerobic Retainer Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A118 Anaerobic Retainer Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |