Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 106 kV/mm | 2700 kV/in | |
Saint-Gobain CHR® 2253-2 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Strength | 106 kV/mm | 2700 kV/in | ASTM D149 |
DuPont Teijin Films Melinex® 329 Polyester Film, 500 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Dielectric Strength | 106 kV/mm | 2700 kV/in | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® EC Polyester Film, 500 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Dielectric Strength | 106 kV/mm | 2700 kV/in | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® EL Polyester Film, 500 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Dielectric Strength | 106 kV/mm | 2700 kV/in | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® MO Polyester Film, 500 Gauge Product Description: Mylar® MO polyester film has excellent electrical properties. This film offer exceptional cut-through resistance, low shrinkage, low moisture absorption, and high thermal durab.. |
|||
Dielectric Strength | 106 kV/mm | 2700 kV/in | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® WC Polyester Film, 500 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Dielectric Strength | 106 kV/mm | 2690 kV/in | |
3M Dyneon™ TFM™ X 1630 PTFE
(discontinued **) Semi-free-flowing resin for convenient handlingHigh bulk density leading to more economical processingVery dense polymer structure; low permeabilityGood electrical and mechanical propertiesSmoother .. |