Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 10.0 kV/mm @Thickness 1.00 mm |
>= 254 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Dielectric Strength | 10.0 - 18.0 kV/mm | 254 - 457 kV/in | Average value: 14.7 kV/mm Grade Count:6 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 30U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | AC 60 Hz; 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in | |
Misumi Alumina 96 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in | |
Misumi Alumina 99 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in | |
Misumi Steatite MgO-SiO2Information provided by MISUMI Corporation. |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.18 mm |
254 kV/in @Thickness 0.125 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 .. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | AC |
Sapco Aluminum Nitride Information provided by Sapco. |
|||
Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in | IEC 60243 |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |
|||
Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in | ASTM-D150 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | ASTM D149 |
Tipco Tipcolite® VASW 150 Phenolic Compound, Glass Fibers & Minerals, Medium-Soft Flow & High Strength |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | |
Covestro Baydur® 60 Polyurethane Rigid integral skin polyurethane foam for engineering components. The integral distribution of density gives a higher flexural modulus. If required, the property level can be improved by increasing .. |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
96hr/105°C+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronit B 66 Phenolic, Paper Reinforcement, Dark Brown, Tubes Description: Specially designed for high-voltage insulation with high requirements for insulating capacity along the tube.Applications: Insulating tubes in high-voltage switchgear and tap changers.... |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Extremely good mechanical properties, at high temperatures. Low thermal conductivity.Applications: Material for components used in the aerospace industry. Insulation parts in wire weldi.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® N196 Paper, 2 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP FR Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relati.. |
|||
Dielectric Strength | 10.0 - 11.0 kV/mm | 254 - 279 kV/in | ASTM D149 |
Adamas Adalon® 452 PTFE, Mica filler Information provided by Adamas, HPM |
|||
Dielectric Strength | >= 10.0 kV/mm @Temperature 90.0 °C |
>= 254 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | |
AGY ADVANTEX® Generic Glass Fiber OC/AGY E-CR glass. Various silanes and starch oil are used as binders. Acid resistant. Lower alkali resistance than VeTron® and ZenTron® glass fibers.Information provided by AGY Holding Corp... |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | Short Time; Dry; ASTM D149 |
Resinoid 2010 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in | |
Beijing Evergrow Resources PTFE Extrusion Tube Features:PTFE extruded tubing is manufactured by high pressure PTFE dispense resin mixed with additive, it is extruded and sintered. According to different demands, the tubing could be opaque or tra.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | Short Time; ASTM D149 |
Plenco 2311 Phenolic, Granular, Transfer Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Dielectric Strength | 10.0 kV/mm | 254 kV/in | 60 Hz, wet, SS; ASTM D149 |
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ.. |
|||
Dielectric Strength | >= 10.0 kV/mm @Thickness 1.00 mm |
>= 254 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6, FR, compliant with ECO protocols, non-brominated, non-chlorinated |